Open any transformer, motor, inductor or AM radio and you will find a magnetic material at its heart — a silicon-steel core, a soft ferrite bead, or the ferrite rod antenna that picks up the broadcast signal. The behaviour of these materials decides how efficiently energy is stored and transferred, and how much of it is wasted as heat. For Wireless PSI and GPSC Electronics, magnetic materials are a high-yield topic: questions on permeability, the hysteresis loop and the soft-versus-hard distinction appear almost every year.
This study note builds from the basic magnetic quantities (H, B, permeability and susceptibility) up to domains, the classification of materials, the B-H hysteresis loop, soft and hard magnetic materials, Curie temperature and core losses. It closes with exam traps and nine practice MCQs with detailed explanations.
1. Basic Magnetic Quantities
Before classifying materials we must fix the language of magnetism. The magnetising force or field intensity H is the applied magnetic field, measured in amperes per metre (A/m). It is the cause. The effect produced inside the material is the magnetic flux density B, measured in tesla (T), which is the total flux per unit area.
The ratio of the two is the permeability of the material:
B = mu × HPermeability links the flux density produced to the applied field
mu = mu0 × murAbsolute permeability as a product of free-space and relative values
Here mu0 is the permeability of free space, a fixed constant equal to 4π × 10-7 H/m (about 1.257 × 10-6 H/m). The dimensionless relative permeability mur = mu / mu0 tells us how many times better than vacuum a material conducts magnetic flux.
Closely related is magnetic susceptibility chi, which measures how easily a material becomes magnetised by H. It links to relative permeability by a simple relation:
chi = mur − 1Susceptibility is one less than relative permeability
The intensity of magnetisation M is the magnetic moment per unit volume induced in the material, and M = chi × H. The sign and size of chi is exactly what we use to sort materials into diamagnetic, paramagnetic and ferromagnetic classes.
2. The Origin of Magnetism
Magnetism in matter comes from moving charge inside atoms. Each electron contributes two magnetic moments: one from its orbital motion around the nucleus, and a larger one from its spin. In most atoms these tiny moments point in random directions and cancel, so the material shows almost no magnetism.
In iron, nickel and cobalt the spins of neighbouring atoms lock together over large regions called magnetic domains. Within a single domain millions of atomic moments already point the same way. In an unmagnetised piece the domains themselves point randomly, so the net effect is zero. Applying H makes favourably-aligned domains grow and rotate; this domain behaviour is what gives ferromagnets their huge permeability and is the physical basis of the hysteresis loop.
3. Classification of Magnetic Materials
Materials are grouped by how their susceptibility responds to an applied field.
Diamagnetic materials
These have mur slightly less than 1 and a small negative susceptibility. They are weakly repelled by a magnetic field. The effect exists in all materials but is masked when stronger effects are present. Examples: copper, bismuth, silver, gold, lead, water.
Paramagnetic materials
These have mur slightly greater than 1 and a small positive susceptibility, so they are weakly attracted. They cannot retain magnetism once the field is removed. Examples: aluminium, platinum, manganese, chromium, oxygen.
Ferromagnetic materials
These have a very large mur (hundreds to many thousands) and a large positive susceptibility. They are strongly attracted and can retain magnetism, which makes permanent magnets possible. Examples: iron, nickel, cobalt, gadolinium and their alloys.
Ferrimagnetic and antiferromagnetic
Two further classes appear in electronics. Ferrimagnetic materials — the ferrites — have opposing atomic moments of unequal size, so a strong net magnetism survives; their high electrical resistivity makes them ideal at high and radio frequencies. Antiferromagnetic materials (such as manganese oxide) have equal and opposite moments that cancel, giving near-zero net magnetism.
| Type | Relative permeability mu_r | Susceptibility sign | Examples |
|---|
| Diamagnetic | Slightly less than 1 | Small negative | Copper, bismuth, silver, gold, water |
| Paramagnetic | Slightly more than 1 | Small positive | Aluminium, platinum, manganese, oxygen |
| Ferromagnetic | Very large (100s-1000s) | Large positive | Iron, nickel, cobalt, gadolinium |
| Ferrimagnetic | Large | Positive | Ferrites (Mn-Zn, Ni-Zn) |
| Antiferromagnetic | About 1 | Small positive | Manganese oxide, chromium |
4. The B-H Hysteresis Loop
If we take an unmagnetised ferromagnetic sample and slowly increase H while plotting B, B rises along a curve and eventually flattens out — this is saturation, where almost all domains are aligned and further H adds little flux.
Now reverse the process. As H is reduced back to zero, B does not return along the same path; some magnetism remains. As H is reversed and cycled, B traces a closed loop called the hysteresis loop. The word hysteresis means "lagging behind" — B lags behind H. Two points on the loop carry the key definitions:
- Retentivity (remanence) Br: the flux density that remains when H is brought back to zero. It measures how much magnetism the material retains on its own.
- Coercivity (coercive force) Hc: the reverse field intensity needed to bring the retained flux density B back to zero. It measures how hard the material resists demagnetisation.
The crucial energy fact: the area enclosed by the loop equals the energy lost as heat per unit volume per cycle. A fat loop wastes a lot of energy; a thin loop wastes little. This loss is the hysteresis loss, and the Steinmetz empirical law estimates it:
Ph = eta × Bmax1.6 × fSteinmetz hysteresis loss; eta is the material constant, B_max the peak flux density, f the frequency
So hysteresis loss rises with frequency and steeply with peak flux density — a vital point for transformer and core design.
5. Soft vs Hard Magnetic Materials
The single most examined distinction in this topic is between soft and hard magnetic materials, decided entirely by the shape of the hysteresis loop.
Soft magnetic materials have a narrow, tall loop: low retentivity, low coercivity, easy to magnetise and demagnetise, and a small loop area meaning low hysteresis loss. They are perfect where the field must reverse rapidly, such as AC cores.
Hard magnetic materials have a wide, fat loop: high retentivity, high coercivity, hard to magnetise and very hard to demagnetise, with a large loop area. They make excellent permanent magnets.
| Property | Soft magnetic | Hard magnetic |
|---|
| Hysteresis loop | Narrow and tall | Wide and fat |
| Retentivity | Low | High |
| Coercivity | Low | High |
| Ease of magnetisation | Easy (and easily demagnetised) | Hard (and hard to demagnetise) |
| Hysteresis loss / loop area | Low (small area) | High (large area) |
| Examples | Silicon (electrical) steel, soft ferrite, permalloy | Alnico, hard ferrite, Nd-Fe-B, carbon steel |
| Typical uses | Transformer and motor cores, electromagnets, inductors | Permanent magnets, loudspeakers, motor field magnets |
Memory hook: Soft = small loop = transformer cores; Hard = huge loop = permanent magnets.
6. Curie Temperature
Heating a ferromagnet shakes its domains. Above a critical temperature called the Curie temperature (or Curie point), thermal agitation destroys the domain alignment, and the material loses its ferromagnetism and becomes paramagnetic. For iron this happens near 770 °C (about 1043 K); for nickel near 358 °C and cobalt near 1130 °C. Cooling below the Curie point restores ferromagnetic behaviour.
7. Core Losses and Why Cores Are Laminated
An AC magnetic core suffers two main losses, together called iron losses or core losses:
- Hysteresis loss — energy lost per cycle equal to the loop area. Reduced by choosing a soft material such as silicon steel with a thin loop.
- Eddy-current loss — the changing flux induces circulating currents inside the conducting core, heating it. Reduced by laminating the core into thin insulated sheets, which break up the current paths, and by adding silicon to raise resistivity.
This is a classic trap: laminations reduce eddy-current loss, not hysteresis loss. Hysteresis loss depends on the material and the loop area, not on whether the core is laminated. At high and radio frequencies even laminations are not enough, so ferrites are used: their very high resistivity makes eddy currents negligible, which is why ferrite cores and ferrite rod antennas dominate RF circuits.
8. Applications in Electronics and Telecom
- Transformer and inductor cores: laminated silicon steel for mains frequencies; ferrite cores for switch-mode supplies and RF.
- Ferrite rod antennas: a soft ferrite rod concentrates the magnetic field of an AM broadcast signal into the coil, used in portable receivers.
- Magnetic recording media: hard magnetic particles store data on tapes and disks because of their high retentivity.
- Loudspeaker and microphone magnets: hard magnets such as Alnico or Nd-Fe-B provide a strong fixed field.
- Relays and electromagnets: soft iron cores that magnetise and release quickly.
9. Exam Tips and Common Mistakes
- Diamagnetic materials have mur less than 1 and are repelled; do not confuse them with paramagnetic (mur just above 1).
- Soft magnetic = narrow loop = low hysteresis loss = cores; hard magnetic = wide loop = high retentivity = permanent magnets.
- Hysteresis loss is proportional to the area of the B-H loop, not its height alone.
- Laminations cut eddy-current loss, not hysteresis loss.
- Above the Curie temperature a ferromagnetic material becomes paramagnetic, not diamagnetic.
- Remember chi = mur − 1 and B = mu H = mu0 mur H.
- B = mu H, mu = mu0 mu_r, and chi = mu_r - 1; mu0 = 4*pi*10^-7 H/m.
- Diamagnetic: mu_r < 1, repelled; paramagnetic: mu_r > 1, weakly attracted; ferromagnetic: mu_r very large, retains magnetism.
- Retentivity is B remaining at H=0; coercivity is the reverse H needed to make B zero.
- Hysteresis loss equals the area of the B-H loop, lost as heat each cycle.
- Soft materials have a narrow loop (low loss) for transformer/motor cores; hard materials have a wide loop (high retentivity) for permanent magnets.
- Above the Curie temperature (iron ~770 C) ferromagnetism is lost and the material turns paramagnetic.
- Laminations and silicon steel cut eddy-current loss; ferrites give very low eddy loss at RF due to high resistivity.
10. Practice MCQs
Test yourself with these nine exam-style questions. Try each before reading the explanation.
Q1. The relative permeability of a diamagnetic material is:
- A.Slightly greater than 1
- B.Slightly less than 1
- C.Very much greater than 1
- D.Exactly zero
Correct Answer: B
Explanation: Diamagnetic materials have mu_r slightly less than 1 and a small negative susceptibility, so they are weakly repelled. Paramagnetics have mu_r slightly above 1; ferromagnetics have mu_r very large.
Q2. Magnetic susceptibility chi is related to relative permeability mu_r by:
- A.chi = mu_r + 1
- B.chi = mu_r - 1
- C.chi = 1 - mu_r
- D.chi = mu_r squared
Correct Answer: B
Explanation: By definition chi = mu_r - 1. For diamagnetics mu_r < 1 gives a negative chi; for paramagnetics and ferromagnetics mu_r > 1 gives a positive chi.
Q3. The area enclosed by the B-H hysteresis loop represents:
- A.Magnetic flux density
- B.Coercive force
- C.Energy lost as heat per cycle per unit volume
- D.Relative permeability
Correct Answer: C
Explanation: The loop area equals the hysteresis loss, the energy dissipated as heat each magnetisation cycle. A wider loop means greater loss, which is why soft cores use thin loops.
Q4. The flux density that remains in a magnetic material when the magnetising force is reduced to zero is called:
- A.Coercivity
- B.Saturation
- C.Retentivity (remanence)
- D.Permeability
Correct Answer: C
Explanation: Retentivity or remanence is the residual B at H = 0. Coercivity is the reverse H needed to reduce that residual B back to zero.
Q5. Which set of properties best describes a SOFT magnetic material?
- A.Wide loop, high retentivity, high coercivity
- B.Narrow loop, low retentivity, low coercivity
- C.Wide loop, low coercivity, high loss
- D.Narrow loop, high coercivity, high loss
Correct Answer: B
Explanation: Soft magnetic materials (silicon steel, soft ferrite, permalloy) have a narrow loop with low retentivity, low coercivity and low hysteresis loss, ideal for transformer and motor cores.
Q6. Above the Curie temperature, a ferromagnetic material becomes:
- A.Diamagnetic
- B.Paramagnetic
- C.Antiferromagnetic
- D.A permanent magnet
Correct Answer: B
Explanation: Thermal agitation above the Curie point (iron ~770 C) destroys domain alignment, so the material loses ferromagnetism and behaves as a weakly attracted paramagnetic material.
Q7. Transformer cores are laminated mainly to reduce:
- A.Hysteresis loss
- B.Copper loss
- C.Eddy-current loss
- D.Dielectric loss
Correct Answer: C
Explanation: Laminating into thin insulated sheets breaks up the circulating currents induced by changing flux, cutting eddy-current loss. Hysteresis loss is reduced by material choice, not lamination.
Q8. A magnetising force H = 500 A/m is applied to a core of relative permeability 800. Taking mu0 = 4*pi*10^-7 H/m, the flux density B is approximately:
- A.0.50 T
- B.0.63 T
- C.0.80 T
- D.1.26 T
Correct Answer: A
Explanation: B = mu0 * mu_r * H = (4*pi*10^-7)(800)(500). mu0*mu_r = 1.005*10^-3; times 500 gives about 0.50 T.
Q9. Ferrites are preferred over silicon steel at high (RF) frequencies because they have:
- A.Higher density
- B.Lower permeability
- C.Very high electrical resistivity, giving low eddy-current loss
- D.A wider hysteresis loop
Correct Answer: C
Explanation: Ferrites are ferrimagnetic with very high resistivity, so eddy currents are negligible at high frequencies. This is why ferrite cores and ferrite rod antennas are standard in RF and switch-mode circuits.